第 34 卷第 2 期 |  | Vol. 34 No. 2 | 2004 年 4 月 | Apr 2004 |
|
所屬欄目:其它
雙季戊四醇重結晶新工藝的研究 |
滕冬成(衡陽(yáng)三化實(shí)業(yè)股份有限公司; 湖南衡陽(yáng)) |
摘 要:研究了一種改進(jìn)的雙季戊四醇重結晶工藝,使雙季戊四醇的灰份從0.1%以上降至0.05%以下,純度從80%提高到85%以上,收率比傳統重結晶工藝提高10%左右,且成本下降,操作更簡(jiǎn)便。實(shí)驗確定的優(yōu)化工藝條件為:溶解水量1:5~6、溶解水溫度60℃、結晶冷卻時(shí)間6~8h、離心分離溫度20℃。 |
關(guān)鍵詞:雙季戊四醇; 灰份; 重結晶; 工藝 |
中圖分類(lèi)號:TQ223.16 文獻標識碼:A 文章編號:1009-9212(2004)02-0053-03 |
|
Study on the New Technology for the Recrystallizaition of Dipentaerythritol |
TENG Tong-cheng (Hengyang sanhua enterprise Inc. Hengyang 421002; China) |
Abstract:A new technology for recrystallized of DPE was studied, the ash cotent of DPE was reduced from 0.1% to 0.05%, the purity of DPE was inproved from 80% to 85%, the total yield is ligher 10% than that old technology. The optimal coditions was follow as :dissolve water multiple 1:5~6: water temperature 60℃;crystallize cooling time 6-8hours; centrifugal temperature 20℃. |
Key words:dipentaerythritol; ash; recrystallize; techlonogy |
|
收稿日期:2003-12-07
|
閱讀全文 |
|